Warm Deformation of Alloy Al – 4.7% Mg – 0.32% Mn – 0.21% Sc – 0.09% Zr


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

The evolution of the structure and mechanical properties of sheets from alloy Al – 4.7% Mg – 0.32% Mn – 0.21% Sc – 0.09% Zr during warm rolling and subsequent annealing is studied. It is shown that extended fibers with a thickness of 50 – 100 nm form inside the deformed grains in the rolling process. Post-rolling annealing of the sheets at 150 and 200°C results in substantial lowering of the elongation after a hold for 3 h; then the ductility recovers after a hold for 5 h. The lowering of the ductility is associated with precipitation of a fine β -phase over grain boundaries during the annealing. The phase grows and its volume fraction decreases when the annealing time is prolonged. The possibility of formation of high-level mechanical properties after warm rolling and subsequent annealing is shown.

Авторлар туралы

A. Pozdnyakov

National Research Technological University “MISiS” (NITU “MISiS”)

Email: barkov@misis.ru
Ресей, Moscow

R. Barkov

National Research Technological University “MISiS” (NITU “MISiS”)

Хат алмасуға жауапты Автор.
Email: barkov@misis.ru
Ресей, Moscow

O. Yakovtseva

National Research Technological University “MISiS” (NITU “MISiS”)

Email: barkov@misis.ru
Ресей, Moscow

V. Levchenko

National Research Technological University “MISiS” (NITU “MISiS”)

Email: barkov@misis.ru
Ресей, Moscow

A. Prosviryakov

National Research Technological University “MISiS” (NITU “MISiS”)

Email: barkov@misis.ru
Ресей, Moscow

V. Zolotorevskii

National Research Technological University “MISiS” (NITU “MISiS”)

Email: barkov@misis.ru
Ресей, Moscow

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Springer Science+Business Media, LLC, part of Springer Nature, 2019