Features of Nonmetallic Inclusion Formation and Evolution During Ladle Treatment and Continuous Casting of Special Alloy Steels


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

Features of nonmetallic inclusion formation and evolution in special alloy steels during ladle treatment and continuous casting are studied for special alloy steel 40Kh. The main differences in types, sizes, and morphology of nonmetallic inclusions in relation to steel deoxidation scheme are analyzed. It is established that the composition of more than 97% of oxide inclusions present belongs to CaO–Al2O3–SiO2, Al2O3–MgO–SiO2, CaO–Al2O3–MgO, CaO–Al2O3–MgO~5% SiO2, Al2O3–MnO–SiO2 systems. The main factors that affect the formation of aluminum-magnesium spinel are determined. It is shown that a non-optimal slag regime in a tundish leads to formation of silicate inclusions with cross section of more than 1000 μm2, even with a steel aluminum content more than 0.015 wt.%.

Авторлар туралы

A. Stepanov

Bardin Central Research Institute of Ferrous Metallurgy (TsNIIchermet)

Хат алмасуға жауапты Автор.
Email: alxstp07@gmail.com
Ресей, Moscow

A. Zaitsev

Bardin Central Research Institute of Ferrous Metallurgy (TsNIIchermet); Faculty of Chemistry, Lomonosov Moscow State University

Email: alxstp07@gmail.com
Ресей, Moscow; Moscow

T. Strizhakova

Bardin Central Research Institute of Ferrous Metallurgy (TsNIIchermet)

Email: alxstp07@gmail.com
Ресей, Moscow

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Springer Science+Business Media New York, 2016