Analysis of Hydrogen Content in the Main Stages of Low-Alloy Aluminum Alloy Flat Ingot Manufacture
- Авторы: Belyaev S.V.1, Kulikov B.P.1, Deev V.B.2, Baranov V.N.1, Rakhuba E.M.2
-
Учреждения:
- Siberian Federal University
- National University of Science and Technology MISiS
- Выпуск: Том 61, № 3-4 (2017)
- Страницы: 325-329
- Раздел: Article
- URL: https://journal-vniispk.ru/0026-0894/article/view/240254
- DOI: https://doi.org/10.1007/s11015-017-0496-7
- ID: 240254
Цитировать
Аннотация
Results are given for research aimed at improving the quality of large tonnage flat ingots under RUSAL Joint Company (Krasnoyarsk) conditions as a result of reducing the hydrogen content within them to less than 0.1 cm3/100g. For this purpose, under production conditions the change in molten aluminum alloys series 1XXX hydrogen content is analyzed in the main stages from the aluminum electrolyzer to the casting machine. Production operations are determined within which there is significant melt impregnation with hydrogen. Research precision is provided by using a developed procedure for molten sample collection in the main production operations and considering the specific nature of production. Technical solutions are proposed from research results aimed at reducing melt hydrogen expansion.
Об авторах
S. Belyaev
Siberian Federal University
Email: kulikov-boris@yandex.ru
Россия, Krasnoyarsk
B. Kulikov
Siberian Federal University
Автор, ответственный за переписку.
Email: kulikov-boris@yandex.ru
Россия, Krasnoyarsk
V. Deev
National University of Science and Technology MISiS
Email: kulikov-boris@yandex.ru
Россия, Moscow
V. Baranov
Siberian Federal University
Email: kulikov-boris@yandex.ru
Россия, Krasnoyarsk
E. Rakhuba
National University of Science and Technology MISiS
Email: kulikov-boris@yandex.ru
Россия, Moscow
Дополнительные файлы