Melting of High-Nitrogen Austenitic Steels at Atmospheric Pressure


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

The article considers conditions for nitrogen bubble formation at the crystallization front for iron and stainless steels. Using the results obtained during plasma-arc remelting, a semi-empirical formula is proposed for calculating maximum permissible nitrogen concentrations. It is shown that during steel crystallization with austenite formation at atmospheric pressure it is possible to obtain dense steel ingots with a nitrogen content exceeding its solubility at the liquidus temperature by a factor of 1.4–1.5.