Influence of the Direction of Propagation of the Main Crack on the Fracture Mechanism upon Impact Bending of Samples of High-Viscous Steel with a Filamentary Structure. Tensile Region


Citar

Texto integral

Acesso aberto Acesso aberto
Acesso é fechado Acesso está concedido
Acesso é fechado Somente assinantes

Resumo

Abstract—The fracture profiles and distribution of the microhardness in regions adjacent to the fracture surface in the region of tension of Charpy samples of the high-viscous 08G2B steel (0.08 C; ~2 Mn; 0.2 Mo; ≈0.15 Σ(Ti–V–Nb); 0.004 N; 0.04 Al; 0.004 S; 0.007 P wt %) with a filamentary structure formed by non-recrystallization controlled rolling with an accelerated cooling have been studied. The factors that provide the extremely high impact toughness of steel in the case of the fracture of the Charpy samples perpendicular to the surface of filaments have been revealed.

Sobre autores

A. Morozova

Mikheev Institute of Metal Physics, Ural Branch, Russian Academy of Sciences

Autor responsável pela correspondência
Email: amorozova@imp.uran.ru
Rússia, Ekaterinburg, 620108

G. Schapov

Ural Federal University Named after the First President of Russia B. N. Yeltsin

Email: amorozova@imp.uran.ru
Rússia, Ekaterinburg, 620002

V. Khotinov

Ural Federal University Named after the First President of Russia B. N. Yeltsin

Email: amorozova@imp.uran.ru
Rússia, Ekaterinburg, 620002

V. Farber

Ural Federal University Named after the First President of Russia B. N. Yeltsin

Email: amorozova@imp.uran.ru
Rússia, Ekaterinburg, 620002

O. Selivanova

Ural Federal University Named after the First President of Russia B. N. Yeltsin

Email: amorozova@imp.uran.ru
Rússia, Ekaterinburg, 620002

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML

Declaração de direitos autorais © Pleiades Publishing, Ltd., 2019