Formation of silicon carbide from microsilica waste by means of lignite semicoke
- Авторы: Anikin A.E.1, Galevskii G.V.1, Rudneva V.V.1
-
Учреждения:
- Siberian State Industrial University
- Выпуск: Том 46, № 2 (2016)
- Страницы: 93-98
- Раздел: Article
- URL: https://journal-vniispk.ru/0967-0912/article/view/178548
- DOI: https://doi.org/10.3103/S0967091216020029
- ID: 178548
Цитировать
Аннотация
The formation of silicon carbide from briquetted batch consisting of microsilica waste from silicon and silicon-alloy production is investigated. The batch is treated at 1873, 1923, and 1973 K, for 5–30 min, with various reducing agents: lignite semicoke, coal semicoke, coke breeze, and coke dust. The best results are obtained when using lignite semicoke from the Berezovsk deposit in Kansko-Achinsk Basin: the yield of silicon carbide is 97.00–97.62%; it constitutes 82.52–84.90% of the products obtained. The optimal treatment temperature and time are determined: 1923–1973 K for 15–20 min. The products consist predominantly of cubic silicon carbide (β SiC). Chemical enrichment increases the SiC content in the products to 90–91%; this is higher than in abrasive micropowder of grain size 1–2 μm. The effectiveness of enrichment in terms of oxide and iron impurities is high: 87–95%. The silicon carbide is characterized by a high silica content: more than 7%. Accordingly, it may be regarded as a promising material for the production of siliconcarbide refractories used in silica binder. Silicon carbide is obtained as micropowder with irregular particles in the size range 0.2–1.0 μm.
Ключевые слова
Об авторах
A. Anikin
Siberian State Industrial University
Автор, ответственный за переписку.
Email: kafcmet@sibsiu.ru
Россия, Novokuznetsk
G. Galevskii
Siberian State Industrial University
Email: kafcmet@sibsiu.ru
Россия, Novokuznetsk
V. Rudneva
Siberian State Industrial University
Email: kafcmet@sibsiu.ru
Россия, Novokuznetsk
Дополнительные файлы