Grain shape as a factor governing the parameters of diamond electroplated coating of dressing tools. Part 2. Actual grain–graphite form contact area and related characteristics as input data for calculating the conditions of diamond electroplated coating application by electroforming method


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

The paper gives experimental data on the actual contact area between grains and the graphite form used in the process of deposition of a diamond coating onto a dressing tool by the electroforming method. Also, the authors provide the results of determination of the maximum section of diamond grains in the powders of different grain sizes, the specific number of grains on the surface and their orientation—the data needed for the calculation of the free surface area of nickel being deposited, and thus the deposition rate and time as well as the final thickness of the diamond electroplated coating.

作者简介

M. Sheiko

Bakul Institute for Superhard Materials

编辑信件的主要联系方式.
Email: max-kiev@i.ua
乌克兰, vul. Avtozavods’ka 2, Kiev, 04074

V. Skok

Bakul Institute for Superhard Materials

Email: max-kiev@i.ua
乌克兰, vul. Avtozavods’ka 2, Kiev, 04074

O. Pasichnyi

Bakul Institute for Superhard Materials

Email: max-kiev@i.ua
乌克兰, vul. Avtozavods’ka 2, Kiev, 04074

补充文件

附件文件
动作
1. JATS XML

版权所有 © Allerton Press, Inc., 2016