Spark Plasma Sintering of Cu-(LaB6-TiB2) Metal-Ceramic Composite and Its Physical-Mechanical Properties


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

A metal-ceramic composite Cu-(LaB6-TiB2) has been produced by the spark plasma sintering. The microstructure, phase composition, mechanical properties and resistivity of the composite are studied. An effective method for reinforcing the interface between the copper matrix and reinforced ceramic particles LaB6-TiB2 has been proposed and implemented. It is demonstrated that consolidation of the metal-ceramic composite by using LaB6-TiB2 particles with naked fibers almost doubles the material's strength. Furthermore, the use of reinforced ceramic particles provides the electrical conductivity on a level with the best materials for resistance-welding electrodes (88% IACS).

作者简介

T. Soloviova

Igor Sikorsky Kyiv Polytechnic Institute

编辑信件的主要联系方式.
Email: tsolov@iff.kpi.ua
乌克兰, pr. Peremohy 37, Kyiv, 03056

I. Solodkyi

Igor Sikorsky Kyiv Polytechnic Institute

Email: tsolov@iff.kpi.ua
乌克兰, pr. Peremohy 37, Kyiv, 03056

P. Loboda

Igor Sikorsky Kyiv Polytechnic Institute

Email: tsolov@iff.kpi.ua
乌克兰, pr. Peremohy 37, Kyiv, 03056

补充文件

附件文件
动作
1. JATS XML

版权所有 © Allerton Press, Inc., 2019