To identify the possible contribution of relaxation processes to the resistance against high-rate deformation, evolution of shock-compression waves in tungsten carbide (WC) ceramics manufactured by spark-plasma sintering at a maximum compressive stress of 27 GPa is measured. Strong elastic precursor decay upon changing the thickness of the samples from 0.15 to 4 mm is revealed. At maximum shock compressive stresses twice exceeding the Hugoniot elastic limit, a decrease in the spall strength value by about 30% from its value in the elastic region is recorded.

Авторлар туралы

A. Savinykh

Institute of Problems of Chemical Physics, Russian Academy of Sciences

Хат алмасуға жауапты Автор.
Email: savas@ficp.ac.ru
Ресей, Chernogolovka, Moscow oblast, 142432

I. Cherepanov

Institute of Problems of Chemical Physics, Russian Academy of Sciences; Moscow State University

Email: savas@ficp.ac.ru
Ресей, Chernogolovka, Moscow oblast, 142432; Moscow, 119991

S. Razorenov

Institute of Problems of Chemical Physics, Russian Academy of Sciences

Email: savas@ficp.ac.ru
Ресей, Chernogolovka, Moscow oblast, 142432

K. Mandel

Freiberg University of Mining and Technology

Email: savas@ficp.ac.ru
Германия, Freiberg, 09599

L. Krüger

Freiberg University of Mining and Technology

Email: savas@ficp.ac.ru
Германия, Freiberg, 09599

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Pleiades Publishing, Ltd., 2019