Temperature and Concentration Dependences of the Electrical Conductivity and Thermal EMF of the PbTe Compound with CdSe Impurities
- Авторлар: Kalmykov R.M.1, Karmokov A.M.1
-
Мекемелер:
- Kabardino-Balkarian State University named after H. M. Berbekov
- Шығарылым: Том 61, № 3 (2018)
- Беттер: 484-490
- Бөлім: Article
- URL: https://journal-vniispk.ru/1064-8887/article/view/240308
- DOI: https://doi.org/10.1007/s11182-018-1423-5
- ID: 240308
Дәйексөз келтіру
Аннотация
The phase composition, electrical conductivity, and thermal EMF coefficient of PbTe with small CdSe impurities are studied, and relationships among these parameters are established. It is shown that the electrical conductivity and thermal EMF coefficient are minimal at the minimal lattice parameter of newly formed phases in the PbTe matrix (at a concentration of 0.5 mole%). A further increase in the concentration leads to the increase of these parameters. Isothermal annealing of the samples leads to an increase in the electrical conductivity and a slight decrease in the thermal EMF.
Авторлар туралы
R. Kalmykov
Kabardino-Balkarian State University named after H. M. Berbekov
Хат алмасуға жауапты Автор.
Email: kalmykov.rustam@yandex.ru
Ресей, Kabardino-Balkarian Republic, Nalchik
A. Karmokov
Kabardino-Balkarian State University named after H. M. Berbekov
Email: kalmykov.rustam@yandex.ru
Ресей, Kabardino-Balkarian Republic, Nalchik
Қосымша файлдар