A synthetic procedure was designed to prepare formulations from Ftorsam-39 monomer (perfluoro-2,5-dimethyl-3,6-dioxanonoic acid triethoxysilylpropylamide) with SKF-26(ONM) fluorine rubber (poly(vinylidene fluoride-co-hexafluoropropylene)) in a presence of AGM-9 (γ-aminopropyltriethoxysilane) as a catalyst and co-reagent. The content of fluorine rubber in the compositions was varied from 10 to 54 wt.%. Thermal properties of the formulations obtained with the ratio Ftorsam-39: SKF-26(ONM): AGM-9 = 40: 54: 6 (wt.%) were assessed using thermomechanical and thermogravimetric analysis and differential scanning calorimetry.

Авторлар туралы

A. Sakharov

N. D. Zelinsky Institute of Organic Chemistry Russian Academy of Science

Email: yar@ioc.ac.ru
Ресей, 47 Leninsky prosp., Moscow, 119991

M. Popovich

N. D. Zelinsky Institute of Organic Chemistry Russian Academy of Science

Email: yar@ioc.ac.ru
Ресей, 47 Leninsky prosp., Moscow, 119991

S. Krukovsky

N. D. Zelinsky Institute of Organic Chemistry Russian Academy of Science

Хат алмасуға жауапты Автор.
Email: yar@ioc.ac.ru
Ресей, 47 Leninsky prosp., Moscow, 119991

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Springer Science+Business Media, LLC, part of Springer Nature, 2019