Research in the Field of Preparing Molded and Unmolded Refractories Based on High-Alumina HCBS. Part 11. Composite Composition HCBS (Fuzed Corundum-Bauxite, Sintered Bauxite, Quartz Glass) and Some Properties of Materials Based Upon Them1
- Authors: Pivinskii Y.E.1, Dyakin P.V.2, Ostryakov L.V.3
-
Affiliations:
- OOO NVF Kerambet-Ogneupor
- FGBOU VPO St. Petersburg State Technological University (Technical University)
- OAO Dinur
- Issue: Vol 58, No 4 (2017)
- Pages: 450-456
- Section: Article
- URL: https://journal-vniispk.ru/1083-4877/article/view/248542
- DOI: https://doi.org/10.1007/s11148-017-0126-8
- ID: 248542
Cite item
Abstract
HCBS of composite composition are prepared by combined wet grinding using fuzed corundum-bauxite containing 93.4% Al2O3 (45%) and sintered Chinese bauxite (45%) as basic materials. The additional component within the composition of the milling charge is very fine quartz glass (10%). The effect of firing temperature in the range 900 – 1600°C on material sintering and mullitization is studied. Values of ultimate strength in bending of 150 MPa are achieved after firing specimens at 1200°C. The material sintering (shrinkage) and mullitization temperature ranges are established.
About the authors
Yu. E. Pivinskii
OOO NVF Kerambet-Ogneupor
Author for correspondence.
Email: pivinskiy@mail.ru
Russian Federation, St. Petersburg
P. V. Dyakin
FGBOU VPO St. Petersburg State Technological University (Technical University)
Email: pivinskiy@mail.ru
Russian Federation, St. Petersburg
L. V. Ostryakov
OAO Dinur
Email: pivinskiy@mail.ru
Russian Federation, Pervoural’sk
Supplementary files