Fabric Deformation During Liquid Treatment in a Roller Washing Machine with a Lengthened Feed Path


Citar

Texto integral

Acesso aberto Acesso aberto
Acesso é fechado Acesso está concedido
Acesso é fechado Somente assinantes

Resumo

The results of a study of deformation of fabrics having a mobile structure during their liquid treatment with a tension are reported. It is shown that acetate fabrics undergo impermissibly high residual deformation when washed in machines with no guide roller drive. Residual deformation of fabrics in hot water can be reduced by 1.6-1.8 times and, at 20°, by 2.2 times by using a controllable guide of fabric transporting rollers.

Sobre autores

E. Martynova

N. E. Bauman Moscow State Technical University

Autor responsável pela correspondência
Email: lizaveta.martynova@gmail.com
Rússia, Moscow

M. Parakhina

Moscow Scientific and Research Institute of Radio Engineering

Email: lizaveta.martynova@gmail.com
Rússia, Moscow

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML

Declaração de direitos autorais © Springer Science+Business Media, LLC, 2017