Formation of Structure of Wear-Resistant Steels 150KhNML and Kh12MFL Upon Quenching
- Authors: Filippov M.A.1, Gervas’ev M.A.1, Plotnikov G.N.2, Zhilin A.S.1, Nikiforova S.M.1
-
Affiliations:
- Ural Federal University after the First President of Russia B. N. Eltsyn
- PromTekhnoTsentr
- Issue: Vol 57, No 11-12 (2016)
- Pages: 641-644
- Section: 90th ANNIVERSARY OF THE DEPARTMENT OF METAL SCIENCE OF THE URAL FEDERAL UNIVERSITY
- URL: https://journal-vniispk.ru/0026-0673/article/view/235232
- DOI: https://doi.org/10.1007/s11041-016-9935-5
- ID: 235232
Cite item
Abstract
The effect of the temperature of heating for quenching on the content of retained austenite and its resistance to the deformation-induced martensitic transformation, the hardening capacity, and the resistance to abrasive wear are studied for high-carbon tool steels 150KhNML and Kh12MFL of pearlitic and ledeburitic classes.
About the authors
M. A. Filippov
Ural Federal University after the First President of Russia B. N. Eltsyn
Author for correspondence.
Email: filma1936@mail.ru
Russian Federation, Ekaterinburg
M. A. Gervas’ev
Ural Federal University after the First President of Russia B. N. Eltsyn
Email: filma1936@mail.ru
Russian Federation, Ekaterinburg
G. N. Plotnikov
PromTekhnoTsentr
Email: filma1936@mail.ru
Russian Federation, Ekaterinburg
A. S. Zhilin
Ural Federal University after the First President of Russia B. N. Eltsyn
Email: filma1936@mail.ru
Russian Federation, Ekaterinburg
S. M. Nikiforova
Ural Federal University after the First President of Russia B. N. Eltsyn
Email: filma1936@mail.ru
Russian Federation, Ekaterinburg
Supplementary files