Abstract

The laws of formation and growth of carbonitride layer in steels 40G2, 38KhMA, 40KhN2MA, and 09GSF at a temperature of 560°C are studied. Metallographic methods are used to determine its composition, location and length. Equations for computing the lengths of the carbonitride phase and of the layer due to surface cyaniding are derived.

About the authors

V. I. Gryzunov

Orsk Liberal-Technological Institute, Branch of the Orsk State University

Email: d33d1@yandex.ru
Russian Federation, Orsk

E. Yu. Priymak

Orsk Liberal-Technological Institute, Branch of the Orsk State University

Email: d33d1@yandex.ru
Russian Federation, Orsk

N. V. Firsova

Orsk Liberal-Technological Institute, Branch of the Orsk State University

Email: d33d1@yandex.ru
Russian Federation, Orsk

T. V. Emel’yanova

“MK ORMETO-YuUMZ” Company

Author for correspondence.
Email: d33d1@yandex.ru
Russian Federation, Orsk

Supplementary files

Supplementary Files
Action
1. JATS XML

Copyright (c) 2017 Springer Science+Business Media, LLC