Crack Resistance of Welded Joints of Pipe Steels of Strength Class K60 of Different Alloying Systems
- Authors: Tabatchikova T.I.1, Tereshchenko N.A.1, Yakovleva I.L.1, Makovetskii A.N.2, Shander S.V.2
-
Affiliations:
- M. N. Mikheev Institute of Metal Physics of the Ural Branch of the Russian Academy of Sciences
- Chelyabinsk Pipe-Rolling Plant, JSC
- Issue: Vol 59, No 11-12 (2018)
- Pages: 767-772
- Section: Welded Joints
- URL: https://journal-vniispk.ru/0026-0673/article/view/236248
- DOI: https://doi.org/10.1007/s11041-018-0224-3
- ID: 236248
Cite item
Abstract
The crack resistance of welded joints of pipe steels of strength class K60 and different alloying systems is studied. The parameter of the crack tip opening displacement (CTOD) is shown to be dependent on the size of the austenite grains and on the morphology of bainite in the superheated region of the heat-affected zone of the weld. The crack resistance is shown to be controllable due to optimization of the alloying system.
About the authors
T. I. Tabatchikova
M. N. Mikheev Institute of Metal Physics of the Ural Branch of the Russian Academy of Sciences
Author for correspondence.
Email: labmet@imp.uran.ru
Russian Federation, Ekaterinburg
N. A. Tereshchenko
M. N. Mikheev Institute of Metal Physics of the Ural Branch of the Russian Academy of Sciences
Email: amakoveckiy@chtpz.ru
Russian Federation, Ekaterinburg
I. L. Yakovleva
M. N. Mikheev Institute of Metal Physics of the Ural Branch of the Russian Academy of Sciences
Email: amakoveckiy@chtpz.ru
Russian Federation, Ekaterinburg
A. N. Makovetskii
Chelyabinsk Pipe-Rolling Plant, JSC
Author for correspondence.
Email: amakoveckiy@chtpz.ru
Russian Federation, Chelyabinsk
S. V. Shander
Chelyabinsk Pipe-Rolling Plant, JSC
Email: amakoveckiy@chtpz.ru
Russian Federation, Chelyabinsk
Supplementary files