Wear (pin-on-disk) tests of low-alloy powder steels (with 0.5 and 0.65% C) are performed after vacuum sintering combined with hardening. The studied alloying systems are 0.65% C + 1.5% Cr + 0.2% Mo, 0.65% C + 0.9% Ni + 0.9% Mo + 0.2% Mn and 0.5% C + 4% Ni + 1.5% Cu + 0.5% Mo. The wear resistance of the steels after the hardening sintering is an order of magnitude higher than after the conventional sintering. The wear resistance of the steels increases in the following order: pearlitic, pearlitic-bainitic, and martensitic structures. Accordingly, the hardness grows from 98 to 105 HRB.

作者简介

R. Bidulský

Technical University of Košice, Faculty of Metallurgy, Department of Metals Forming

编辑信件的主要联系方式.
Email: robert.bidulsky@tuke.sk
斯洛伐克, Košice

J. Bidulská

Technical University of Košice, Faculty of Metallurgy, Department of Metals Forming

Email: robert.bidulsky@tuke.sk
斯洛伐克, Košice

M. Grande

Politecnico di Torino, Department of Applied Science and Technology

Email: robert.bidulsky@tuke.sk
意大利, Alessandria

补充文件

附件文件
动作
1. JATS XML

版权所有 © Springer Science+Business Media New York, 2017