Tantalum nitrides are synthesized by ammonolysis of a mesoporous magnesiothermic tantalum powders. The effect of specific surface area of the powders and synthesis temperature on product composition is shown. Nitrogen content in the ammonolysis product of tantalum powder with a specific surface area of 56 m2 g–1 corresponds to oxynitride TaON exposed to 600°C for 1 h. The specific surface area of the oxynitride is 35 m2 g–1.
About the authors
V. M. Orlov
Tananaev Institute of Chemistry and Technology of Rare Elements and Mineral Raw Materials
Author for correspondence.
Email: orlov@chemy.kolasc.net.ru
Russian Federation, Apatity, 184209
V. Ya. Kuznetsov
Tananaev Institute of Chemistry and Technology of Rare Elements and Mineral Raw Materials
Email: orlov@chemy.kolasc.net.ru
Russian Federation, Apatity, 184209
R. N. Osaulenko
Petrozavodsk State University
Email: orlov@chemy.kolasc.net.ru
Russian Federation, Petrozavodsk, Republic of Karelia, 185910
Supplementary files