Reduction of Silicon from a Ceramic Mold during Directional Solidification of Single-Crystal Nickel Superalloys
- Authors: Min P.G.1, Sidorov V.V.1, Vadeev V.E.1
- 
							Affiliations: 
							- All-Russia Institute of Aviation Materials (VIAM)
 
- Issue: Vol 2018, No 13 (2018)
- Pages: 1288-1292
- Section: Processes of Manufacture of Ferrous and Nonferrous Metals
- URL: https://journal-vniispk.ru/0036-0295/article/view/172840
- DOI: https://doi.org/10.1134/S0036029518130177
- ID: 172840
Cite item
Abstract
Silicon is one of the most harmful impurities in nickel superalloys used for casting aviation turbines: it decreases the high-temperature strength and the ductility. The reduction of silicon from a ceramic mold is experimentally studied during the directional solidification of a single-crystal nickel superalloy.
About the authors
P. G. Min
All-Russia Institute of Aviation Materials (VIAM)
							Author for correspondence.
							Email: viamlab3@mail.ru
				                					                																			                												                	Russian Federation, 							Moscow						
V. V. Sidorov
All-Russia Institute of Aviation Materials (VIAM)
														Email: viamlab3@mail.ru
				                					                																			                												                	Russian Federation, 							Moscow						
V. E. Vadeev
All-Russia Institute of Aviation Materials (VIAM)
														Email: viamlab3@mail.ru
				                					                																			                												                	Russian Federation, 							Moscow						
Supplementary files
 
				
			 
					 
						 
						 
						 
						 
				 
  
  
  
  
  Email this article
			Email this article  Open Access
		                                Open Access Access granted
						Access granted Subscription Access
		                                		                                        Subscription Access
		                                					