Heat-Engineering Characteristics of Diatomaceous-Earth Materials in a Wide Temperature Range
- Authors: Prikhod’ko E.V.1, Kinzhibekova A.K.1, Karmanov A.E.1, Nikiforov A.S.1
-
Affiliations:
- S. Toraigyrov Pavlodar State University
- Issue: Vol 75, No 1-2 (2018)
- Pages: 60-62
- Section: Coatings
- URL: https://journal-vniispk.ru/0361-7610/article/view/244909
- DOI: https://doi.org/10.1007/s10717-018-0029-2
- ID: 244909
Cite item
Abstract
The ultimate strength of diatomite in compression was studied as a function of temperature in the range 50 – 700°C. The ultimate strength in compression at temperature 450 – 500°C is approximately a factor of 2 greater than the strength under normal conditions. This makes it possible to organize the process of heating diatomite-based lining of high-temperature furnaces more efficiently.
About the authors
E. V. Prikhod’ko
S. Toraigyrov Pavlodar State University
Email: aleke4599@mail.ru
Kazakhstan, Pavlodar
A. K. Kinzhibekova
S. Toraigyrov Pavlodar State University
Email: aleke4599@mail.ru
Kazakhstan, Pavlodar
A. E. Karmanov
S. Toraigyrov Pavlodar State University
Email: aleke4599@mail.ru
Kazakhstan, Pavlodar
A. S. Nikiforov
S. Toraigyrov Pavlodar State University
Author for correspondence.
Email: aleke4599@mail.ru
Kazakhstan, Pavlodar
Supplementary files