Kinetics of photodegradation of alizarin green in an acoustic fluidized bed using TiO2 catalyst


Citar

Texto integral

Acesso aberto Acesso aberto
Acesso é fechado Acesso está concedido
Acesso é fechado Somente assinantes

Resumo

The kinetics of photodegradation of alizarin green (AG) in an acoustic fluidized bed was investigated using Degussa P25 catalyst and N-doped TiO2 catalyst, respectively. The effects of initial concentration of AG, catalyst amount, initial pH value and liquid flow rate on the photodegradation rates were the main goal of present study. The degradation rate increased with increasing amount of photocatalyst, pH value and liquid flow rate, reached a maximum and then decreased. The degradation rate decreased with increasing initial concentration. According to the Langmuir–Hinshelwood model, the disappearance of the AG followed pseudo-first-order kinetics. Experimental results showed that AG can be degraded effectively by Degussa P25 catalyst and N-doped TiO2 catalyst in an acoustic fluidized bed reactor. N-doped TiO2 catalyst has high and significant photocatalytic activity and in comparison with Degussa P25 catalyst was photocatalyst.

Sobre autores

C. Si

Jining University

Autor responsável pela correspondência
Email: chongdiansi@126.com
República Popular da China, Qufu

J. Zhou

Department of Energy and Material Engineering

Email: chongdiansi@126.com
República Popular da China, Jining

Y. Sun

Jining University

Email: chongdiansi@126.com
República Popular da China, Qufu

G. Liu

Jining University

Email: chongdiansi@126.com
República Popular da China, Qufu

H. Gao

Jining University

Email: chongdiansi@126.com
República Popular da China, Qufu

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML

Declaração de direitos autorais © Allerton Press, Inc., 2016