Tellurium Solubility in TlGaTe2 and TlInTe2 and the Electrophysical Properties of Solid Solutions
- Autores: Nadzhafov A.I.1,2, Alieva N.A.2, Khalilova K.G.1
-
Afiliações:
- Institute of Physics
- Institute of Radiation Problems
- Edição: Volume 60, Nº 9 (2018)
- Páginas: 1698-1703
- Seção: Dielectrics
- URL: https://journal-vniispk.ru/1063-7834/article/view/203752
- DOI: https://doi.org/10.1134/S1063783418090226
- ID: 203752
Citar
Resumo
The complex methods of the physicochemical analysis are used to study TlGaTe2–Te and TlInTe2–Te alloys in which the tellurium solubility region up to 5.0 at % is observed. The temperature dependences of the lattice parameters and the electrical conductivity of TlGaTe2 + x and TlInTe2 + x have been studied in different crystallographic directions. The TlGaTe2 + x and TlInTe2 + x solid solutions undergo a phase transition at a temperature of 498 K. The transition nature is interpreted.
Sobre autores
A. Nadzhafov
Institute of Physics; Institute of Radiation Problems
Autor responsável pela correspondência
Email: a.najafov@mail.ru
Azerbaijão, Baku, AZ1143; Baku, AZ1143
N. Alieva
Institute of Radiation Problems
Email: a.najafov@mail.ru
Azerbaijão, Baku, AZ1143
K. Khalilova
Institute of Physics
Email: a.najafov@mail.ru
Azerbaijão, Baku, AZ1143
Arquivos suplementares