The Influence of Corundum Content and Sintering Temperature on the Mechanical Properties of CaO–ZrO2–Al2O3 Ceramic Composites


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

We have studied the mechanical properties (Vickers microhardness HV and fracture toughness KC) of nanostructured CaO–ZrO2–Al2O3 ceramic composites as dependent on the content of corundum (0 ≤ \(C_{Al_{2}O_{3}}\) ≤ 25%) and the temperature of sintering (1250°C ≤ T1 ≤ 1500°C). Optimum value of the corundum content (\(C_{Al_{2}O_{3}}\) = 5%) and optimum regime (T1 = 1300°C, 5 min; T2 = 1200°C, 4 h) of two-stage sintering are established, which favor attaining the best mechanical characteristics of ceramic composites (HV = 12.25 GPa, KC = 8.47 MPa m1/2).

作者简介

A. Dmitrievskii

Tambov State University

编辑信件的主要联系方式.
Email: aadmitr@yandex.ru
俄罗斯联邦, Tambov, 392000

A. Tyurin

Tambov State University

Email: aadmitr@yandex.ru
俄罗斯联邦, Tambov, 392000

A. Zhigachev

Tambov State University

Email: aadmitr@yandex.ru
俄罗斯联邦, Tambov, 392000

D. Guseva

Tambov State University

Email: aadmitr@yandex.ru
俄罗斯联邦, Tambov, 392000

P. Ovchinnikov

Tambov State University

Email: aadmitr@yandex.ru
俄罗斯联邦, Tambov, 392000

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2018