The Influence of Corundum Content and Sintering Temperature on the Mechanical Properties of CaO–ZrO2–Al2O3 Ceramic Composites
- Autores: Dmitrievskii A.A.1, Tyurin A.I.1, Zhigachev A.O.1, Guseva D.G.1, Ovchinnikov P.N.1
-
Afiliações:
- Tambov State University
- Edição: Volume 44, Nº 2 (2018)
- Páginas: 141-144
- Seção: Article
- URL: https://journal-vniispk.ru/1063-7850/article/view/207275
- DOI: https://doi.org/10.1134/S1063785018020219
- ID: 207275
Citar
Resumo
We have studied the mechanical properties (Vickers microhardness HV and fracture toughness KC) of nanostructured CaO–ZrO2–Al2O3 ceramic composites as dependent on the content of corundum (0 ≤ \(C_{Al_{2}O_{3}}\) ≤ 25%) and the temperature of sintering (1250°C ≤ T1 ≤ 1500°C). Optimum value of the corundum content (\(C_{Al_{2}O_{3}}\) = 5%) and optimum regime (T1 = 1300°C, 5 min; T2 = 1200°C, 4 h) of two-stage sintering are established, which favor attaining the best mechanical characteristics of ceramic composites (HV = 12.25 GPa, KC = 8.47 MPa m1/2).
Sobre autores
A. Dmitrievskii
Tambov State University
Autor responsável pela correspondência
Email: aadmitr@yandex.ru
Rússia, Tambov, 392000
A. Tyurin
Tambov State University
Email: aadmitr@yandex.ru
Rússia, Tambov, 392000
A. Zhigachev
Tambov State University
Email: aadmitr@yandex.ru
Rússia, Tambov, 392000
D. Guseva
Tambov State University
Email: aadmitr@yandex.ru
Rússia, Tambov, 392000
P. Ovchinnikov
Tambov State University
Email: aadmitr@yandex.ru
Rússia, Tambov, 392000
Arquivos suplementares