Electrical Conductivity of Carbon Materials Based on Coal-Tar Pitch with Added Graphite Foam


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

Attention focuses on the structure and electrical conductivity of carbon materials produced by the carbonization (at 900°C) of coal-tar pitch with the addition of 0.03–0.3% graphite foam and oxidized graphite foam. In these quantities, the additives do not change the X-ray diffraction characteristics but considerably increase the conductivity of the product over the whole temperature range. With increase in concentration of the additives, the conductivity of the carbon material increases. At room temperature, it is 14–20 S/cm, which is at least 2–3 times the value in the absence of the additives. The influence on the conductivity is greater for the oxidized graphite foam. This may be attributed to the smaller size of the crystallites and the greater distance between the planes, resulting in greater accessible surface area of the graphite layers orienting the pitch molecules on carbonization.

Авторлар туралы

Ch. Barnakov

Institute of Coal Chemistry and Materials Chemistry, Federal Research Center of Coal and Coal Chemistry, Siberian Branch

Хат алмасуға жауапты Автор.
Email: barnakov@rambler.ru
Ресей, Kemerovo

G. Khokhlova

Institute of Coal Chemistry and Materials Chemistry, Federal Research Center of Coal and Coal Chemistry, Siberian Branch

Email: barnakov@rambler.ru
Ресей, Kemerovo

A. Popova

Institute of Coal Chemistry and Materials Chemistry, Federal Research Center of Coal and Coal Chemistry, Siberian Branch

Email: barnakov@rambler.ru
Ресей, Kemerovo

A. Romanenko

Institute of Inorganic Chemistry, Siberian Branch

Email: barnakov@rambler.ru
Ресей, Novosibirsk

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Allerton Press, Inc., 2018