Production of high-carbon ferrochrome from dry-quenched semicoke
- Авторы: Strakhov V.M.1, Medyanik V.S.2, Malinovskaya L.I.2, Tsernikel A.A.3, Veselovsky I.A.3
-
Учреждения:
- Kuznetsk Center
- Leninsk-Kuznetsk Semicoking Plant
- Serov Ferro-Alloy Plant
- Выпуск: Том 59, № 7 (2016)
- Страницы: 254-259
- Раздел: Coal and Coke
- URL: https://journal-vniispk.ru/1068-364X/article/view/226008
- DOI: https://doi.org/10.3103/S1068364X16070061
- ID: 226008
Цитировать
Аннотация
The quenching of semicoke by saturated steam (heating-gas temperature 550°C) is described. The working-moisture content Wr in the semicoke is 3.0–6.7% for the new quenching method. As a reducing agent, semicoke has good characteristics: relatively low ash content (Ad = 7.1%), low sulfur content (Sd = 0.13%) and phosphorus content (Pd = 0.029%), and high reactivity (\({K_{C{O_2}}}\) = 4.0 cm3/g s) and electrical resistivity (ρ > 1.9 × 106 Ω cm). In tests, dry-quenched semicoke performs well in the production of high-carbon ferrochrome: decreased power consumption; increased furnace productivity; decreased consumption of chromium ore; and decreased sulfur content in the ferrochrome when Karaganda coal is completely reduced by the semicoke. The optimal semicoke content in the batch is up to 50 kg.
Ключевые слова
Об авторах
V. Strakhov
Kuznetsk Center
Автор, ответственный за переписку.
Email: vuhin2013@yandex.ru
Россия, ul. Klimasenko 19, Novokuznetsk, 654040
V. Medyanik
Leninsk-Kuznetsk Semicoking Plant
Email: vuhin2013@yandex.ru
Россия, ul. Voikova 1, Leninsk-Kuznetsk, 652515
L. Malinovskaya
Leninsk-Kuznetsk Semicoking Plant
Email: vuhin2013@yandex.ru
Россия, ul. Voikova 1, Leninsk-Kuznetsk, 652515
A. Tsernikel
Serov Ferro-Alloy Plant
Email: vuhin2013@yandex.ru
Россия, ul. Nakhabina 1, Serov, 624992
I. Veselovsky
Serov Ferro-Alloy Plant
Email: vuhin2013@yandex.ru
Россия, ul. Nakhabina 1, Serov, 624992
Дополнительные файлы