Production of high-carbon ferrochrome from dry-quenched semicoke
- Autores: Strakhov V.M.1, Medyanik V.S.2, Malinovskaya L.I.2, Tsernikel A.A.3, Veselovsky I.A.3
-
Afiliações:
- Kuznetsk Center
- Leninsk-Kuznetsk Semicoking Plant
- Serov Ferro-Alloy Plant
- Edição: Volume 59, Nº 7 (2016)
- Páginas: 254-259
- Seção: Coal and Coke
- URL: https://journal-vniispk.ru/1068-364X/article/view/226008
- DOI: https://doi.org/10.3103/S1068364X16070061
- ID: 226008
Citar
Resumo
The quenching of semicoke by saturated steam (heating-gas temperature 550°C) is described. The working-moisture content Wr in the semicoke is 3.0–6.7% for the new quenching method. As a reducing agent, semicoke has good characteristics: relatively low ash content (Ad = 7.1%), low sulfur content (Sd = 0.13%) and phosphorus content (Pd = 0.029%), and high reactivity (\({K_{C{O_2}}}\) = 4.0 cm3/g s) and electrical resistivity (ρ > 1.9 × 106 Ω cm). In tests, dry-quenched semicoke performs well in the production of high-carbon ferrochrome: decreased power consumption; increased furnace productivity; decreased consumption of chromium ore; and decreased sulfur content in the ferrochrome when Karaganda coal is completely reduced by the semicoke. The optimal semicoke content in the batch is up to 50 kg.
Palavras-chave
Sobre autores
V. Strakhov
Kuznetsk Center
Autor responsável pela correspondência
Email: vuhin2013@yandex.ru
Rússia, ul. Klimasenko 19, Novokuznetsk, 654040
V. Medyanik
Leninsk-Kuznetsk Semicoking Plant
Email: vuhin2013@yandex.ru
Rússia, ul. Voikova 1, Leninsk-Kuznetsk, 652515
L. Malinovskaya
Leninsk-Kuznetsk Semicoking Plant
Email: vuhin2013@yandex.ru
Rússia, ul. Voikova 1, Leninsk-Kuznetsk, 652515
A. Tsernikel
Serov Ferro-Alloy Plant
Email: vuhin2013@yandex.ru
Rússia, ul. Nakhabina 1, Serov, 624992
I. Veselovsky
Serov Ferro-Alloy Plant
Email: vuhin2013@yandex.ru
Rússia, ul. Nakhabina 1, Serov, 624992
Arquivos suplementares