Effect of Operational Factors on Steel-Teeming Ladle Lining Working Layer Life
- 作者: Kondrukevich A.A.1, Ryabyi D.V.2
-
隶属关系:
- FGOU VO D. I. Mendeleev Russian Chemical technology University
- GBUZ DonGTU
- 期: 卷 58, 编号 5 (2018)
- 页面: 469-474
- 栏目: Article
- URL: https://journal-vniispk.ru/1083-4877/article/view/248891
- DOI: https://doi.org/10.1007/s11148-018-0129-0
- ID: 248891
如何引用文章
详细
Reasons are considered for crack formation in periclase-carbon, aluminopericlase-carbon and spinel-periclase-carbon refractories, and also partial effect on life of flux-cored wire and inert gas blowing intensity in enterprises smelting low-alloy, carbon, and low-silicon materials. The turnover of a steel-teeming ladle is more than 4 – 5 melts/day: the proportion of melts treated in FLU is 100%; open stream casting into a CBCM. Defining factors and the proportion of their effect on steel-teeming ladle life are evaluated from the results of this work.
作者简介
A. Kondrukevich
FGOU VO D. I. Mendeleev Russian Chemical technology University
编辑信件的主要联系方式.
Email: kondrukevich@list.ru
俄罗斯联邦, Moscow
D. Ryabyi
GBUZ DonGTU
Email: kondrukevich@list.ru
乌克兰, Lisichansk
补充文件