Research in the Field of Preparing Molded and Unmolded Refractories Based on High-Alumina HCBS. Part 11. Composite Composition HCBS (Bauxite Electrocorundum, Quartz Glass) and some Properties of Materials Based Upon Them1
- Авторлар: Pivinskii Y.E.1, Dyakin P.V.2, Ostryakov L.V.3
-
Мекемелер:
- OOO NVF Kerambet-Ogneupor
- FGBOU VPO St. Petersburg State Technological University (Technical University)
- OAO Dinur
- Шығарылым: Том 58, № 5 (2018)
- Беттер: 514-520
- Бөлім: Article
- URL: https://journal-vniispk.ru/1083-4877/article/view/248901
- DOI: https://doi.org/10.1007/s11148-018-0135-2
- ID: 248901
Дәйексөз келтіру
Аннотация
Single-stage wet grinding is used to prepare composite composition HCBS based on bauxite, electrocorundum, and very fine fuzed quartz with a moisture content of 11%. Properties are studied for specimens fired in the range 900 – 1640°C. Depending on firing temperature Tfir three typical ranges are separated corresponding to primary sintering and shrinkage (up to 1200°C), mullitization and growth (1200 – 1400°C), and sintering of mullitized material (above 1400°C). The maximum value of ultimate strength in bending of 140 – 150 MPa corresponds to Tfir = 1250 – 1400°C and in compression 750 MPa at 1640°C.
Негізгі сөздер
Авторлар туралы
Yu. Pivinskii
OOO NVF Kerambet-Ogneupor
Хат алмасуға жауапты Автор.
Email: pivinskiy@mail.ru
Ресей, St. Petersburg
P. Dyakin
FGBOU VPO St. Petersburg State Technological University (Technical University)
Email: pivinskiy@mail.ru
Ресей, St. Petersburg
L. Ostryakov
OAO Dinur
Email: pivinskiy@mail.ru
Ресей, Pervoural’sk
Қосымша файлдар