Resistance of Refractories of the Al2O3–Cr2O3 System Under Liquid-Phase Reduction Conditions of Iron-Containing Technogenic Waste

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

Results are provided for a laboratory study of the applicability of refractories in the Al2O3–Cr2O3 system in bubble-agitated double-chamber laboratory furnaces during processing of a broad spectrum of iron-containing materials, including technogenic waste. Laboratory tests are conducted for refractory life in a medium of molten iron. Conditions are modeled for exploitation of a refractory in melting and reducing zones of a bubble-agitated type furnace. Optical microscopy is used to study zones and the overall depth of crucible reaction with melt at the melt – refractory crucible interface.

作者简介

G. Podgorodetskii

FGAOU VO NITU MISiS

Email: axelrodlev@yandex.ru
俄罗斯联邦, Moscow

L. Aksel’rod

FGAOU VO NITU MISiS

编辑信件的主要联系方式.
Email: axelrodlev@yandex.ru
俄罗斯联邦, Moscow

E. Agapov

FGAOU VO NITU MISiS

Email: axelrodlev@yandex.ru
俄罗斯联邦, Moscow

T. Erokhov

FGAOU VO NITU MISiS

Email: axelrodlev@yandex.ru
俄罗斯联邦, Moscow

V. Gorbunov

FGAOU VO NITU MISiS

Email: axelrodlev@yandex.ru
俄罗斯联邦, Moscow

K. Sankin

FGAOU VO NITU MISiS

Email: axelrodlev@yandex.ru
俄罗斯联邦, Moscow

补充文件

附件文件
动作
1. JATS XML

版权所有 © Springer Science+Business Media, LLC, part of Springer Nature, 2018