Permeable Ceramic with Three-Fraction Electromelted Corundum Filler and Porcelain Binder
- Авторы: Belyakov A.V.1, Oo Z.Y.1, Popova N.A.1, Min Y.A.1
-
Учреждения:
- D. I. Mendeleev Russian Chemical Technology University
- Выпуск: Том 59, № 4 (2018)
- Страницы: 391-394
- Раздел: Article
- URL: https://journal-vniispk.ru/1083-4877/article/view/249096
- DOI: https://doi.org/10.1007/s11148-018-0242-0
- ID: 249096
Цитировать
Аннотация
Porous permeable materials are prepared by selecting the grain size composition with electromelted corundum filler and porcelain mix PFL-1 binder. Specimens with an improved set of properties are prepared with addition to the composition of 5 wt.% porcelain binder (above 100% filler) after firing at 1450°C. Specimen ultimate strength in bending is 14.6 MPa, open porosity 44%, and gas permeability coefficient 0.85 μm2.
Об авторах
A. Belyakov
D. I. Mendeleev Russian Chemical Technology University
Автор, ответственный за переписку.
Email: av_bel@bk.ru
Россия, Moscow
Zaw Oo
D. I. Mendeleev Russian Chemical Technology University
Email: av_bel@bk.ru
Россия, Moscow
N. Popova
D. I. Mendeleev Russian Chemical Technology University
Email: av_bel@bk.ru
Россия, Moscow
Ye Min
D. I. Mendeleev Russian Chemical Technology University
Email: av_bel@bk.ru
Россия, Moscow
Дополнительные файлы