Corrosion Testing of Baddeleyite-Corundum and Chromium Oxide Materials in Aluminum Phosphate Glass Melts


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

The significance of the question of corrosion and erosion resistance for refractory materials in direct heating electric furnaces for vitrification of highly active waste (HAW) is substantiated. Algorithms are provided for evaluating their resistance to action of phosphate melts under electric furnace operating conditions. Comparative corrosion tests are performed for refractory materials surpassing Bk-33 objects with respect to quality in melts of aluminophosphate glass with simulation of HAW. Tests results are valuable for selecting lining material in planning ÉP-500 type vitrification electric furnaces with a prolonged service life, and also the next generation of moveable and small-scale melting units.

Авторлар туралы

M. Remizov

FGUP PO Mayak

Email: kozlov_pavel@inbox.ru
Ресей, Ozersk, Chelyabinsk Region

P. Kozlov

FGUP PO Mayak; Ozersk Technological Institute (branch of FGAOU VO National Research Nuclear University MIFI)

Хат алмасуға жауапты Автор.
Email: kozlov_pavel@inbox.ru
Ресей, Ozersk, Chelyabinsk Region; Ozersk, Chelyabinsk Region

A. Kazadaev

FGUP PO Mayak

Email: kozlov_pavel@inbox.ru
Ресей, Ozersk, Chelyabinsk Region

V. Medvedev

Ozersk Technological Institute (branch of FGAOU VO National Research Nuclear University MIFI)

Email: kozlov_pavel@inbox.ru
Ресей, Ozersk, Chelyabinsk Region

V. Malinkovich

Glass Furnace Solutions Co.

Email: kozlov_pavel@inbox.ru
Ресей, Moscow

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Springer Science+Business Media, LLC, part of Springer Nature, 2018