Intensification of Sulfide Copper-Nickel Ore Heap Leaching with Bioreagent-Oxidant Participation


Cite item

Full Text

Open Access Open Access
Restricted Access Access granted
Restricted Access Subscription Access

Abstract

With the aim of intensification, improving economic efficiency, and controlling sulfide ore heap bacterial leaching features and leaching regimes are studied for lean copper-nickel ore with the participation of a bioreagent-oxidant prepared by iron-oxidizing micro-organisms and concentrated adsorption immobilization in a separate reactor. Research established the ore size for heap leaching and an increase in metal extraction with an increase in bioreagent concentration. Use of the heap bioleaching technology developed for ore with a size of –10 mm containing 0.32% nickel and 0.11% copper makes it possible to increase nickel extraction into solution to 6.3–19.5% and copper to 5.8–24.2% with consumption of sulfuric acid lower by 4.4–14.6% compared with use of seeding ore with bacteria.

About the authors

Zheng Zhihong

East China Technological University (ECUST)

Author for correspondence.
Email: ecitzhzheng76@126.com
China, Nanchang

L. N. Krylova

National University of Science and Technology MISiS

Email: ecitzhzheng76@126.com
Russian Federation, Moscow

D. A. Ryabtsev

Engineering Center, Moscow Institute of Physics and Technology (State University)

Email: ecitzhzheng76@126.com
Russian Federation, Moscow

Supplementary files

Supplementary Files
Action
1. JATS XML

Copyright (c) 2016 Springer Science+Business Media New York