With the aim of intensification, improving economic efficiency, and controlling sulfide ore heap bacterial leaching features and leaching regimes are studied for lean copper-nickel ore with the participation of a bioreagent-oxidant prepared by iron-oxidizing micro-organisms and concentrated adsorption immobilization in a separate reactor. Research established the ore size for heap leaching and an increase in metal extraction with an increase in bioreagent concentration. Use of the heap bioleaching technology developed for ore with a size of –10 mm containing 0.32% nickel and 0.11% copper makes it possible to increase nickel extraction into solution to 6.3–19.5% and copper to 5.8–24.2% with consumption of sulfuric acid lower by 4.4–14.6% compared with use of seeding ore with bacteria.

作者简介

Zheng Zhihong

East China Technological University (ECUST)

编辑信件的主要联系方式.
Email: ecitzhzheng76@126.com
中国, Nanchang

L. Krylova

National University of Science and Technology MISiS

Email: ecitzhzheng76@126.com
俄罗斯联邦, Moscow

D. Ryabtsev

Engineering Center, Moscow Institute of Physics and Technology (State University)

Email: ecitzhzheng76@126.com
俄罗斯联邦, Moscow

补充文件

附件文件
动作
1. JATS XML

版权所有 © Springer Science+Business Media New York, 2016