Optimum operating-temperature range and lifetime estimate for ZnSb:0.1 at % Cu thermoelectrics
- Авторлар: Prokofieva L.V.1, Nasredinov F.S.2, Konstantinov P.P.1, Shabaldin A.A.1
-
Мекемелер:
- Ioffe Institute
- Peter the Great St. Petersburg Polytechnic University
- Шығарылым: Том 51, № 8 (2017)
- Беттер: 1012-1016
- Бөлім: XV International Conference “Thermoelectrics and Their Applications—2016”, St. Petersburg, November 15–16, 2016
- URL: https://journal-vniispk.ru/1063-7826/article/view/200856
- DOI: https://doi.org/10.1134/S1063782617080267
- ID: 200856
Дәйексөз келтіру
Аннотация
The temperature dependences of concentration and mobility are investigated in 300–700–300 K thermal cycles at different durations of low-temperature annealing of a ZnSb:0.1 at % Cu sample before the onset of every thermal cycle. Concurrently, the material is annealed for 1500 hours at a temperature difference of 310–670 K, and, then, its thermoelectric parameters are measured. The results are analyzed taking into account the features of the crystalline structure and the covalent nature of the chemical bonds in ZnSb. The operating range and lifetime of this composition are estimated on the basis of a model of the interaction of impurity defects with a decrease in their acceptor activity and an increase in the hole-scattering cross section at low temperatures.
Авторлар туралы
L. Prokofieva
Ioffe Institute
Хат алмасуға жауапты Автор.
Email: lprokofieva496@gmail.com
Ресей, St. Petersburg, 194021
F. Nasredinov
Peter the Great St. Petersburg Polytechnic University
Email: lprokofieva496@gmail.com
Ресей, St. Petersburg, 195251
P. Konstantinov
Ioffe Institute
Email: lprokofieva496@gmail.com
Ресей, St. Petersburg, 194021
A. Shabaldin
Ioffe Institute
Email: lprokofieva496@gmail.com
Ресей, St. Petersburg, 194021
Қосымша файлдар