The kinetics of electrical damage (breakdown) of polymer films 20–50 μm thick in a constant-sign field of 0.5–0.6 GV/m at 77–300 K has been studied. At elevated temperatures (250–300 K), the exponential temperature dependence of the durability and the above-barrier thermal-fluctuation mechanism of electron emission from traps, i.e., space charge accumulation leading to breakdown, take place. At low temperatures (77–200 K), there are separate local decreases in the durability (minima) at the athermal durability level. The identity of the temperatures of durability minima and measured thermoluminescence maxima of polymers was found. A conclusion is made about the mechanism of thermally stimulated tunneling (subbarrier emission) of electrons from traps.

Авторлар туралы

A. Slutsker

Ioffe Physical-Technical Institute

Хат алмасуға жауапты Автор.
Email: Alexander.Slutsker@mail.ioffe.ru
Ресей, ul. Politekhnicheskaya 26, St. Petersburg, 194021

T. Veliev

Abdullaev Institute of Physics

Email: Alexander.Slutsker@mail.ioffe.ru
Әзірбайжан, pr. H. Javid 33, Baku, Az-1143

I. Alieva

Abdullaev Institute of Physics

Email: Alexander.Slutsker@mail.ioffe.ru
Әзірбайжан, pr. H. Javid 33, Baku, Az-1143

V. Alekperov

Abdullaev Institute of Physics

Email: Alexander.Slutsker@mail.ioffe.ru
Әзірбайжан, pr. H. Javid 33, Baku, Az-1143

Yu. Polikarpov

Peter the Great Saint-Petersburg Polytechnic University

Email: Alexander.Slutsker@mail.ioffe.ru
Ресей, ul. Politekhnicheskaya 29, St. Petersburg, 195251

D. Karov

Peter the Great Saint-Petersburg Polytechnic University

Email: Alexander.Slutsker@mail.ioffe.ru
Ресей, ul. Politekhnicheskaya 29, St. Petersburg, 195251

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Pleiades Publishing, Ltd., 2016