Limiting State of High-Speed Drills


Cite item

Full Text

Open Access Open Access
Restricted Access Access granted
Restricted Access Subscription Access

Abstract

Drill failure is due to the predominant wear of the rear surface or ribbon, depending on the range of cutting speed. Such wear is accompanied by increase in the cutting torque to critical values. Formulas are derived for the limiting permissible wear.