Achievement the strength level of 2400-2500 MPa in the ХН3МФС-type steels with different carbon contents
- Authors: Vylezhnev V.P.1, Sukhikh A.A.1, Simonov Y.N.1, Dementev V.B.1
-
Affiliations:
- Issue: No 1 (2014)
- Pages: 6-13
- Section: MATERIAL SCIENCE
- URL: https://journal-vniispk.ru/1994-6309/article/view/302188
- ID: 302188
Cite item
Full Text
Abstract
Keywords
About the authors
V. P. Vylezhnev
Ph.D. (Engineering), Associate Professor, Perm National Research Polytechnic University
A. A. Sukhikh
Scientific Associate, Institute of Mechanics Ural Branch of Russian Academy of Sciences
Y. N. Simonov
Email: simonov@pstu.ru
D.Sc. (Engineering), Professor, Perm National Research Polytechnic University, e-mail: simonov@pstu.ru
V. B. Dementev
D.Sc. (Engineering), Institute of Mechanics Ural Branch of Russian Academy of Sciences
References
- Вылежнев В.П., Коковякина С.А., Симонов Ю.Н. Сухих А.А. Повышение характеристик надежности мартенситно-стареющей стали 03Н18К9М5Т путем создания структуры типа «Нанотриплекс» // МиТОМ. - 2010. - №11. - С. 39-47.2. Курдюмов Г.В., Утевский Л.М., Энтин Р.И. Превращения в железе и стали. - М.: Наука, 1977. - 236 с.3. Дементьев В.Б. Перспективы применения совмещенных процессов деформации и термической обработки для обеспечения эксплуатационной надежности деталей // Сб. науч. труд. ОКТБ «Восход», г. Ижевск, Ижевский Механич. ин-т. - 1989. - №1. - С.3-16.4. Быкова П.О., Заяц Л.Ц., Панов Д.О. Выявление границ аустенитных зерен в сталях с мартенситной структурой методом окисления // Заводская лаборатория. Диагностика материалов. - 2008. - №6. - С.42-45.
Supplementary files