Materials Based on Solid Solutions of Bismuth and Antimony Tellurides Formed by Rapid Melt Crystallization Methods

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

p-type Bi0.5Sb1.5Te3 solid solutions prepared by hot pressing and the extrusion of powders prepared by rapid melt crystallization methods such as melt spinning and melt crystallization in a liquid are investigated. The morphology of the powders, the sample cleavage surface, and their microstructure are investigated using optical microscopy, scanning electron microscopy, and scanning tunneling microscopy. The mechanical properties of the samples are investigated by room-temperature compression tests. The Seebeck coefficient, electrical conductivity, and thermal conductivity of the materials are measured in the temperature range of 100–600 K. The highest limiting compressive strength σB = 145 MPa at 300 K and maximal thermoelectric efficiency (ZT)max = 1.34 at 370 K are found for materials extruded from granules prepared by melt crystallization in water and ground in a ball mill.

作者简介

L. Ivanova

Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences

编辑信件的主要联系方式.
Email: ivanova@imet.ac.ru
俄罗斯联邦, Moscow, 119334

Yu. Granatkina

Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences

Email: ivanova@imet.ac.ru
俄罗斯联邦, Moscow, 119334

A. Malchev

Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences

Email: ivanova@imet.ac.ru
俄罗斯联邦, Moscow, 119334

I. Nikhezina

Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences

Email: ivanova@imet.ac.ru
俄罗斯联邦, Moscow, 119334

M. Emel’yanov

Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences

Email: ivanova@imet.ac.ru
俄罗斯联邦, Moscow, 119334

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2019